Mild Two-Step Thermochemical Recovery of Clean Glass Fibers from Wind-Blade GFRP.
AbdulAziz AlGhamdi, Imtiaz Ali, Salman Raza Naqvi
Abstract
Open AccessEnd-of-life wind turbine blade accumulation is a growing global materials management problem and current industrial recycling routes for glass fiber-reinforced polymer composites remain limited in material recovery value. There is limited understanding on how to recover clean glass fibers while keeping thermal exposure and energy input low, and existing studies have not quantified whether very short isothermal thermal residence can still result in complete matrix removal. The hypothesis of this study is that a mild two-step thermochemical sequence can recover clean glass fibers at lower temperature and near zero isothermal dwell if pyrolysis and oxidation are separated. We used wind-blade epoxy-based GFRP in a step-batch reactor and combined TGA-based thermodynamic mapping, short pyrolysis at 425 °C, and mild oxidation at 475 °C with controlled dwell from zero to thirty minutes. We applied model-free kinetics and machine learning methods to quantify activation energy trends as a function of conversion. The thermal treatment of 425 °C for zero minutes in nitrogen, followed by 475 °C for fifteen minutes in air, resulted in mechanically sound, visually clean white fibers. These fibers retained 76% of the original tensile strength and 88% of the Young's modulus, which indicates the potential for energy-efficient GFRP recycling. The activation energy was found to be approximately 120 to 180 kJ mol-1. These findings demonstrate energy lean recycling potential for GFRP and can inform future industrial scale thermochemical designs.