Effect of Laser Pulse Width on Cutting Quality and Efficiency in CFRP: Mechanism and Optimization.
Chunmeng Chen, Long Chen, Guojun Zhang, Yu Huang, Huijuan Ma, Youmin Rong
Abstract
Open AccessThis study systematically investigates the influence of laser pulse duration on cutting efficiency, heat-affected-zone (HAZ) formation, and mechanical integrity during carbon fiber-reinforced polymer (CFRP) laser cutting. Three distinct pulse-width lasers-picosecond, nanosecond, and quasi-continuous-wave (QCW)-are compared. Results show that pulse duration governs material removal mechanisms and HAZ extent: the nanosecond laser achieves the smallest HAZ and minimal porosity; the picosecond laser exhibits limited thermal accumulation due to low average power; and the QCW laser induces the largest HAZ (11.6 times that of the nanosecond laser) and significant porosity. Cutting efficiency scales inversely with pulse width, with single-hole processing times of 480.4 s for picosecond-laser cutting, 76.8 s for nanosecond-laser cutting, and 4.028 s for QCW-laser cutting, reflecting a transition from thermal ablation to mechanical spallation. Mechanical testing reveals that while tensile and flexural strengths vary by less than 5% across laser types, damage morphology and failure modes differ significantly. In situ digital image correlation (DIC) and 3D CT imaging show that longitudinal plies fail via fiber pull-out, whereas transverse plies fail via interfacial debonding. QCW-laser-cut specimens exhibit more uniform strain distribution and higher damage tolerance. An optimized process parameter is proposed: nanosecond-laser cutting at 200 W and 20 kHz achieves a HAZ of less than 50 µm and a cutting time of less than 80 s, offering the best balance between efficiency and quality.